MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Adamas Adalon® 403 PTFE, 15% Polyimide
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 - 1.98 g/cc1.90 - 1.98 g/ccASTM D792
Deformation 7.0 - 13 %7.0 - 13 %ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57 - 6457 - 64ASTM D2240
Ball Indentation Hardness 48.0 - 52.0 MPa6960 - 7540 psiISO 2032-N132
Tensile Strength at Break >= 16.0 MPa>= 2320 psiASTM D4745-97
Elongation at Break >= 180 %>= 180 %ASTM D4745-97
Compressive Strength 6.50 - 8.50 MPa
@Temperature 23.0 °C,
Time 86400 sec
943 - 1230 psi
@Temperature 73.4 °F,
Time 24.0 hour
@ 1% deformation, 140 Kg/cm2; ASTM D621
Coefficient of Friction, Dynamic 0.10 - 0.150.10 - 0.15ASTM D1894
Coefficient of Friction, Static 0.18 - 0.420.18 - 0.42ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+18 ohm-cm8.00e+18 ohm-cmASTM D257
Surface Resistance 6.00e+14 ohm6.00e+14 ohmASTM D257
Dielectric Constant 1.8
@Frequency 60.0 - 2.00e+6 Hz
1.8
@Frequency 60.0 - 2.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 - 50.0 kV/mm508 - 1270 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FASTM C 177
Melting Point 327 °C621 °FDSC
Maximum Service Temperature, Air 250 °C482 °FDSC
Minimum Service Temperature, Air -85.0 °C-121 °FDSC
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Adamas Adalon® 463 PTFE, 15% Special Polyimide
Fluorseals PTFE Unfilled
Adamas Adalon® 266 PTFE, Mineral/Glass Bubbles Filler
Adamas Adalon® 415 PTFE, 10% Organic Filler

PHADAM029 / 147215

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.