MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Information provided by FIBERFIL Engineered Plastics, now an A. Schulman product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Water Absorption 0.020 %0.020 %24 hr; ASTM D570
Linear Mold Shrinkage  0.010 cm/cm
@Thickness 3.17 mm
0.010 in/in
@Thickness 0.125 in
ASTM D955
 0.012 cm/cm
@Thickness 6.35 mm
0.012 in/in
@Thickness 0.250 in
ASTM D955
Melt Flow 7.0 g/10 min7.0 g/10 min230/2.16 (typical); ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80 - 8580 - 85ASTM D785
Tensile Strength, Yield 27.6 MPa4000 psiASTM D638
Elongation at Yield 30 %30 %ASTM D638
Tensile Modulus 2.48 GPa360 ksiASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790
Flexural Modulus 2.34 GPa340 ksiTangent; ASTM D790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C180 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 199 - 210 °C390 - 410 °F
Middle Barrel Temperature 204 - 227 °C400 - 440 °F
Front Barrel Temperature 182 - 199 °C360 - 390 °F
Nozzle Temperature 182 - 193 °C360 - 380 °F
Melt Temperature 199 - 232 °C390 - 450 °F
Mold Temperature 32.2 - 71.1 °C90.0 - 160 °F
Drying Temperature 76.7 °C170 °FDrying not normally required
Dry Time 2 hour2 hourDrying not normally required
Moisture Content <= 0.20 %<= 0.20 %recommended for molding
Back Pressure 0.000 - 0.689 MPa0.000 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized
A. Schulman Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc
A. Schulman TPP20AC06HB 20% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene

PFIBFIL20 / 38205

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.