MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 66 GF 30 TS Polyamide 66, 30% Glass Fiber, Thermal Stabilization
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Features

PA 66 for injection moulding, chemically reinforced with 30% glass fiber, heat stabilized, suitable for high strength and high impact mouldings. Used in the automotive, engineering and electrical industry. Can be used in environment, in which long time heat impact of up to 150°C occurs. Decrease in tensile strength by 50% after 5000 hours at 170°C. The heat stabilization predetermines the products to an environment with long time heat exposure, like intake pipes, cylinder heads, induction coils, carrying parts in the motor fixing in the motor area. Application: hobby tools, gears, covers of electric tools, cooling water distribution in the automotive industry. Delivered in black.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0074 cm/cm0.0074 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0115 cm/cm0.0115 in/inSTN 64 0808
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psiSTN EN ISO 527-2
Elongation at Break 3.0 %3.0 %STN EN ISO 527-2
Tensile Modulus 9.50 GPa1380 ksiSTN EN ISO 527-2
Flexural Strength 225 MPa32600 psiSTN EN ISO 178
Flexural Modulus 7.40 GPa1070 ksiSTN EN ISO 178
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -20.0 °C
23.8 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmSTN IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmSTN IEC 60093
Dielectric Strength 40.0 kV/mm1020 kV/inSTN IEC 60243
Comparative Tracking Index 400 V400 VSTN 34 6468
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC; STN EN ISO 3146
Maximum Service Temperature, Air 170 °C338 °Flong term 5000h; STN EN ISO 527-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FSTN EN ISO 75/A
Vicat Softening Point 250 °C482 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled
DSM Fibre Intermediates Nyrim® 1500 (Dry)
Domo TECHNYL® eXten D 218CR V33 BLACK Nylon Blend, PA 6.10, 66, Dry
Domo TECHNYL® eXten D 218CR V33 BLACK Nylon Blend, PA 6.10, 66, Conditioned

PPLACO046 / 106924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.