MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ex-Tech Plastics VersaTech™ APET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.

Characteristics:
Transparent
Exceptional visual properties
Superior performance in critical consumer applications

End Uses:
Food and medical trays
Consumer packaging: clamshell, blister and tray

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Viscosity Measurement >= 0.75>= 0.75Intrinsic Viscosity; ASTM D3835
Linear Mold Shrinkage 0.020 - 0.050 cm/cm0.020 - 0.050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.6 MPa8500 psiASTM D638
Elongation at Break 250 %250 %
Flexural Modulus 2.41 GPa350 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 240 °C>= 464 °F
 
Optical PropertiesMetricEnglishComments
Haze <= 2.0 %<= 2.0 %ASTM D1003
Transmission, Visible >= 90 %>= 90 %ASTM D1003
 
Descriptive Properties
Clarity>99%ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Spartech APET SP4110 Copolyester Sheet
Celanese Rynite® 408 NC010 PET
Envalior Arnite® A02 307 PET
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)

PEXTEC992 / 133217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.