MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Heat-Away™ 638 Thermally Conductive Grease, Aluminum Nitride Filled
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Aremco's Heat-Away™ thermal greases are ceramic and metal-filled silicone systems which offer exceptional thermal and electrical properties to 550 ºF. These materials are used in high-power electronic devices, heat pipes, and other heat exchange systems.

Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.27 g/cc2.27 g/cc
Solids Content 100 %100 %
Water Absorption 0.00 %0.00 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 11.8 kV/mm300 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.23 W/m-K15.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Descriptive Properties
Chemical ResistanceExcellent
ColorGray
FillerAluminum Nitride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil G-9020 Silicone Grease
Aremco Heat-Away™ 637 Thermally Conductive Grease, Alumina Filled
Lord Adhesives Thermoset™ TC-228 Thermally Conductive Grease
Lord Adhesives Thermoset™ TC-350 Thermally Conductive Silicone Grease
2-Octanol, C8H18O

PAREM27 / 24291

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.