MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

JIS SK5 Water Hardening Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Water-Hardening Steel

Material Notes: JIS tool steels SK3M, SK5M, SK6M, SK7M, SK1, SK2, SK3, SK4, SK5, SK6, and SK7 differ only in carbon specification; SKC3 includes a vanadium max spec.

Key Words: JIS G4401(83) SK5. Comparable to SK3M, SK5M, SK6M, SK7M, SK1, SK2, SK3, SK4, SK6, SK7, SKC3, AISI W1 Tool Steel, UNS T72301
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³(AISI W1)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 207<= 207
Modulus of Elasticity 205 GPa29700 ksi(AISI W1)
Poissons Ratio 0.280.28(AISI W1)
Shear Modulus 80.0 GPa11600 ksi(AISI W1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000300 ohm-cm0.0000300 ohm-cm(AISI W1)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 20.0 - 100 °C
5.78 µin/in-°F
@Temperature 68.0 - 212 °F
(AISI W1)
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
(AISI W1)
 13.8 µm/m-°C
@Temperature 0.000 - 500 °C
7.67 µin/in-°F
@Temperature 32.0 - 932 °F
(AISI W1)
Specific Heat Capacity 0.461 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
(AISI W1)
Thermal Conductivity 48.0 W/m-K333 BTU-in/hr-ft²-°F(AISI W1)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 345 °C347 - 653 °FTempering Temperature (AISI W1)
 760 - 845 °C1400 - 1550 °FHardening Temperature (AISI W1)
Annealing Temperature 740 - 790 °C1360 - 1450 °F(AISI W1)
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.80 - 0.90 %0.80 - 0.90 %
Chromium, Cr <= 0.30 %<= 0.30 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 97.3 - 99.2 %97.3 - 99.2 %As Balance
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.35 %<= 0.35 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
JIS SK5M Water Hardening Tool Steel
JIS S45C Steel, Normalized
JIS SKD11 Tool Steel
LG Chemical AF342 ABS, Flame Retardant
304 Stainless Steel

MSTZJSK5 / 231123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.