MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Flam™ 0803 LDPE NH Yellow Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes:

Features:

  • Flame Retardant
  • Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.06 g/cc0.0383 lb/in³ASTM D792
    Water Absorption 0.020 %0.020 %at Equilibrium; ASTM D570
    Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM D955
    Melt Flow 1.37 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    1.37 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 8888ASTM D2240
    Tensile Strength, Ultimate 8.07 MPa1170 psiASTM D638
    Elongation at Break 1000 %1000 %ASTM D638
    Flexural Strength 5.17 MPa750 psiASTM D790
    Flexural Modulus 0.185 GPa26.8 ksiMethod I (3 point load), Procedure B); ASTM D790
    Izod Impact, Notched 3.84 J/cm7.20 ft-lb/in73°F; ASTM D256
    Gardner Impact 14.35 J10.58 ft-lbASTM D3029
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 1.80e+15 ohm-cm1.80e+15 ohm-cmASTM D257
    Dielectric Constant  2.64
    @Frequency 100000 Hz
    2.64
    @Frequency 100000 Hz
    ASTM D150
     3.15
    @Frequency 100 Hz
    3.15
    @Frequency 100 Hz
    ASTM D150
    Dielectric Strength 26.0 kV/mm661 kV/inASTM D149
    Dissipation Factor  0.015
    @Frequency 100000 Hz
    0.015
    @Frequency 100000 Hz
    ASTM D150
     0.016
    @Frequency 100 Hz
    0.016
    @Frequency 100 Hz
    ASTM D150
     
    Thermal PropertiesMetricEnglishComments
    Flammability, UL94  V-0
    @Thickness 2.20 mm
    V-0
    @Thickness 0.0866 in
     V-0
    @Thickness 3.17 mm
    V-0
    @Thickness 0.125 in

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Multibase Multi-Flam™ 0803 LDPE NH Polyethylene
    Multibase Multi-Flam™ 2903 LDPE Polyethylene
    Techmer ES Plastiblend® LDPE E FR V-2
    Cheng Yu Plastic PE221 Flame Retardant LDPE
    Avient Maxxam™ FR PE126 BLK 3330 Polyethylene, Low Density (LDPE)

    PMULTI285 / 54189

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.