MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exterex™ NP451 Synthetic Fluid
Categories: Fluid; Lubricant

Material Notes: Product Description: Esterex™ Polyol Esters are API category Group V fluids. Esterex™ Polyol Esters have excellent lower-temperature properties, good lubricating properties and low volatilities. Esterex™ Polyol Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal for use in highly loaded, high-speed lubricant applications where energy efficiency is desired.

Appearance: Bright & Clear

Availability: Asia Pacific, Central America, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc
@Temperature 15.6 °C
0.0337 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 130130Index; ASTM D2270
Kinematic Viscosity 7610 cSt
@Temperature -40.0 °C
7610 cSt
@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 25 cSt25 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.0 cSt5.0 cStASTM D445
Evaporation Loss 6.0 %
@Temperature 205 °C,
Time 23400 sec
6.0 %
@Temperature 401 °F,
Time 6.50 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.0100.010[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesMetricEnglishComments
Pour Point -60.0 °C-76.0 °FASTM D5950/D97
Flash Point 245 °C473 °FPMCC; ASTM D92
 255 °C491 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.45061.4506ASTM D1218
 
Descriptive Properties
Aniline Point<68°FASTM D611
Biodegradation (%)83.6OECD 301F
Color<0.5ASTM D1500
CompositionWater<500 ppm, ASTM D6304 (mod)
Density Correction Factor0.00076 (g/cc)/°CASTM D1250
Elastomer Compatibility (%)-11Nitrile Hardness Change, ASTM D471
 12.7Fluoroelastomer Volume Change, ASTM D471
 -15Polyacrylate Hardness Change, ASTM D471
 -15.9Fluoroelastomer Tensile Strength Change, ASTM D471
 -22.9Fluoroelastomer Elongation Change, ASTM D471
 25Nitrile Volume Change, ASTM D471
 -36.2Polyacrylate Elongation Change, ASTM D471
 -36.4Nitrile Elongation Change, ASTM D471
 -39.2Polyacrylate Tensile Strength Change, ASTM D471
 -47.8Nitrile Tensile Strength Change, ASTM D471
 51.2Polyacrylate Volume Change, ASTM D471
 -8Fluoroelastomer Hardness Change, ASTM D471
Fire Point549°FCOC, ASTM D92
Hydrolytic Stability, TAN Change0.17 mg KOH/gASTM D2619
Kauri-Butanol Value72ASTM D1133
Noack Volatility (%)4.6ASTM D5800/DIN 51581
RPVOT240 minNeat, ASTM D2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow UCON™ LB-65 Fluids and Lubricants
ChevronTexaco 5606G Aircraft Hydraulic Oil
Anderol ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22
Phillips 66 32 Super Hydraulic Oil

PEX99704 / 175940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.