MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A808 HSLA Steel, Thickness 50 - 65 mm (2 to 2.5 in.)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel

Material Notes: HSLA (High-strength low-alloy) steels are used for their higher strength and atmospheric corrosion resistance. They can be considered to be microalloyed steel and are designed for mechanical rather than compositional specs. ASTM A808 is noted for good Charpy impact strength at low temperatures and is used in railway cars.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 414 MPa>= 60000 psiVaries with size and form
Tensile Strength, Yield >= 290 MPa>= 42000 psiVaries with size and form
Elongation at Break >= 18 %>= 18 %in 200 mm (8 in.); Varies with size and form
 >= 22 %>= 22 %in 50 mm (2 in.); Varies with size and form
Modulus of Elasticity 205 GPa29700 ksiTypical of steel
Poissons Ratio 0.280.28Calculated
Shear Modulus 80.0 GPa11600 ksiTypical of steel
Charpy Impact 40.0 - 60.0 J
@Temperature -45.0 °C
29.5 - 44.3 ft-lb
@Temperature -49.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Iron, Fe >= 97.3 %>= 97.3 %As Balance
Manganese, Mn <= 1.65 %<= 1.65 %
Nb + V <= 0.15 %<= 0.15 %
Niobium, Nb (Columbium, Cb) 0.020 - 0.10 %0.020 - 0.10 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.50 %0.15 - 0.50 %
Sulfur, S <= 0.050 %<= 0.050 %
Vanadium, V <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A808 HSLA Steel, Thickness < 40 mm (1.5 in.)
AISI Type S24100 Stainless Steel 25 mm annealed bar at RT
ASTM A808 HSLA Steel, Thickness 40 - 50 mm (1.5 to 2 in.)
AISI Type 651 (19-9 DL) Stainless Steel warm worked and stress relieved
AISI Type 651 (19-9 DL) Stainless Steel cold drawn and stress relieved

MSA808C / 14063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.