MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Heraeus Clevios™ S V4 Antistatic/Conductive Polymer Coating for Screen Printing
Categories: Polymer

Material Notes: Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Clevios™ S V4 is the high conductivity screen printing paste grade. Used for transparent electrodes for EL lamps, touch panels, membrane switches, and printed electronics. Features include flexibility, transparency, high conductivity, and 3-D thermoformability.

Information provided by Heraeus, Conductive Polymers Division.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 3500 - 4500 cP3500 - 4500 cPAs Supplied
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 250 - 300 ohm250 - 300 ohmprints from standard 140/31 screen
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 5.00 - 30.0 °C
6.00 Month
@Temperature 41.0 - 86.0 °F
in unopened original container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Heraeus Clevios™ S V3 Antistatic/Conductive Polymer Coating for Screen Printing
Heraeus Clevios™ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ S HT Antistatic/Conductive Polymer Coating for Screen Printing
Heraeus Clevios™ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Conductive Sulfonate Polymer for Antistatic Coatings

PHERA984 / 149973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.