MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Talcoprene® 1540TLT 1 Talc-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Special Grades Talcoprene® 40% Talc-Reinforced Polypropylene, heat stab, low fogging

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Water Absorption 0.050 %
@Temperature 23.0 °C,
Time 86400 sec
0.050 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inSO.F.TER Method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7272ASTM D785
Tensile Strength 30.0 MPa4350 psiASTM D638
Flexural Strength 49.0 MPa7110 psiASTM D790
Flexural Modulus 3.70 GPa537 ksiASTM D790
Izod Impact, Notched 0.260 J/cm0.487 ft-lb/inASTM D256/A
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Constant 2.52.5ASTM D150
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 90.0 µm/m-°C38.9 - 50.0 µin/in-°FASTM D696
Vicat Softening Point 93.0 °C199 °F50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Fortron® 1140 L6 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese SO.F.TER Talcoprene® 1520TL Talc-Reinforced Polypropylene
Celanese SO.F.TER Talcoprene® 1540TL Talc-Reinforced Polypropylene
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber

PSOFS846 / 162310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.