MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, plus superior thermal performance to resist blistering during lead-free SMT processes.

Color stability is enhanced compared to previous flame-retarded grades. Quick crystallization in water-cooled molds allows for fast cycle times using mold temperatures as low as 150°F (65°C).

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/ccASTM D792
Moisture Absorption at Equilibrium 0.10 %0.10 %24 hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 178 MPa25800 psiASTM D638
Elongation at Yield 1.7 %1.7 %ASTM D638
Tensile Modulus 14.2 GPa2060 ksiASTM D638
Flexural Strength 257 MPa37300 psiASTM D790
Flexural Modulus 14.1 GPa2050 ksiASTM D790
Poissons Ratio 0.370.37
Shear Modulus 5.18 GPa751 ksiCalculated
Shear Strength 70.0 MPa10200 psiASTM D732
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 326 °C619 °FASTM D3418

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® LF-1950 HS NT-9 PPA, 50% Long Glass Fiber Reinforced, Conditioned
Syensqo (Solvay Specialty Polymers) Amodel® LF-1930 HS NT-9 PPA, 30% Long Glass Fiber Reinforced, Conditioned
Syensqo (Solvay Specialty Polymers) Amodel® LF-1630 L NT-7 PPA, 30% Long Carbon Fiber Reinforced, Dry
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, at 50% RH
RTP Company RTP 4099 X 94115 Polyphthalamide (PPA); Impact Modified - Glass Fiber - Heat Stabilized

PSOLVT67 / 21363

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.