MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Iupilon® ECF 2030R Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: 30% carbon fiber. Carbon fiber reinforced (flame retardant) grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics. Superior impact strength. Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC. Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Water Absorption 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
Immersion
Linear Mold Shrinkage, Flow 0.00010 - 0.0015 cm/cm
@Thickness 3.20 mm
0.00010 - 0.0015 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiISO 527-1,2
Elongation at Break 3.0 %3.0 %ISO 527-1,2
Tensile Modulus 17.2 GPa2490 ksiISO 527-1,2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 16.2 GPa2350 ksiISO 178
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179-1,2
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179-1,2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Deflection Temperature at 0.46 MPa (66 psi) 152 °C306 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FISO 75-1,2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Albis Plastics ALCOM PC 740 GF23 PTFE 5 , 23% Glass Fiber; 5% PTFE
Mitsubishi Iupilon® CFH 2010 Polycarbonate
Trinseo PULSE™ 2000 ABS + PC
LG Chemical Lupoy 1302-10 Polycarbonate Resin

PMITSU9279 / 191952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.