MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.

Applications: stretched film and tapes for production of high strength knitted & wovens.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ISO 1183
Melt Flow  1.8 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 27 g/10 min
@Load 21.6 kg,
Temperature 190 °C
27 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 868
Tensile Strength at Break 32.0 MPa4640 psiISO 527
Tensile Strength, Yield 21.0 MPa3050 psiISO 527
Elongation at Break >= 1000 %>= 1000 %ISO 527
Elongation at Yield 10 %10 %ISO 527
Tensile Modulus 0.800 GPa116 ksiISO 527
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Softening Point 73.0 °C163 °FISO 306
Brittleness Temperature >= -80.0 °C>= -112 °FASTM D746-72
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 280 °C392 - 536 °F
 
Descriptive Properties
Flexural Creep Modulus (MPa)9004 point, 1 min; DIN 19537-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) 7000F High Density Polyethylene
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene
Iran Petrochemical (PCC) Arak BL2 HDPE
Iran Petrochemical (PCC) Arak BL3 HDPE

PIPC204 / 149666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.