MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Röchling Durostone® EPC 203 Reinforced Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Durostone® EPC 203 is a tissue-fiber reinforced plastic. It is characterized by good mechanical and electrical properties and meets the thermal class F.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 350 MPa50800 psiParallel; ISO 527
Modulus of Elasticity 23.0 GPa3340 ksiPerpendicular; ISO 178
Flexural Strength 450 MPa65300 psiPerpendicular; ISO 178
Compressive Strength 500 MPa72500 psiPerpendicular; ISO 604
Izod Impact, Notched (ISO) 100 kJ/m²47.6 ft-lb/in²Parallel; ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  2.76 kV/mm
@Temperature 90.0 °C
70.0 kV/in
@Temperature 194 °F
Parallel; IEC 60243
 16.0 kV/mm
@Temperature 90.0 °C
406 kV/in
@Temperature 194 °F
Perpendicular; EC 60243
Comparative Tracking Index 180 V180 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 - 20.0 µm/m-°C5.56 - 11.1 µin/in-°F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FISO 8302
Maximum Service Temperature, Air 155 °C311 °FThermal Endurance; TI, IEC 60216
 
Descriptive Properties
Colorgreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Solvay CYCOM® 754 Epoxy Resin with 36% - HS - 200 – 300; 75°C Cure
Röchling Glastic® EPC 205 Reinforced Epoxy Resin
Röchling Durostone® EPM 203 Reinforced Epoxy Resin

PROCH9079 / 232782

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.