MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman Llumar E1220 SR CDF (Silver) Window Film
Categories: Polymer; Film

Material Notes: Low-E film provides superior energy conservation by reducing winter heat loss through windows. It is scratch-resistant, shields 99% of ultraviolet rays, reduces glare, and has the highest heat rejection performance of all LLumar films. It is suitable for commercial and residential applications where summer and winter energy control are major concerns.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 12 %12 %
UV Transmittance 9.0 %9.0 %Solar
Reflection Coefficient, Visible (0-1) 0.570.57Total Solar Reflectance
 0.620.62Visible Reflectance (exterior)
 0.650.65Visible Reflectance (interior)
 
Descriptive Properties
% Glare Reduction87
% Summer Solar Heat Gain Reduction80
% Total Solar Energy Rejected83
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction25
Emissivity0.38
Light to solar gain (LSG)0.71
Shading coefficient0.19
Solar absorption34
Solar Heat Gain Coefficient0.17
U-value0.78Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK 85-5-5-5 Cast UNS C83600 Bearing Bronze
Ampco Metal AMPCO® 642 Aluminum-Silicon-Copper Alloy, Hot Extruded (M-30), > 4"
Miracll E355D Thermoplastic Polyurethane (TPUR), Polyester Grade

PEATM5420 / 222614

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.