MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oceanchem Group Sodium Bromide (NaBr)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: NaBr

Cas No.: 7647-15-6

Use: Mainly used as completion fluid, mounting fluid and maintaining fluid in oil drilling. Applied to the production of film, medicine, spice, dyestuff, etc.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 5.5 - 8.05.5 - 8.050 g/L
Molecular Weight 102.89 g/mol102.89 g/mol
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %Pharm Grade
 <= 0.50 %<= 0.50 %Industrial Grade
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 0.50 %0.50 %Pharm Grade
 1.0 %1.0 %Industrial Grade
Iron, Fe <= 0.00040 %<= 0.00040 %Pharm Grade
 <= 0.00050 %<= 0.00050 %Industrial Grade
Lead, Pb <= 0.00040 %<= 0.00040 %Pharm Grade
 <= 0.00050 %<= 0.00050 %Industrial Grade
 
Descriptive Properties
BrO3- (%)0.003Pharm Grade
 0.005Industrial Grade
CAS Number7647-15-6
Iodine, I (%)<0.006Pharm Grade
 <0.01Industrial Grade
Molecular FormulaNaBr
NaBr (%)98.5Industrial Grade
 99Pharm Grade
SO42- (%)0.01Pharm Grade
 0.02Industrial Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sodium Bromide, NaBr
Mateck Sodium Chloride (NaCl)
Mateck Window Grade Zinc Selenide, ZnSe
Zinc Selenide, ZnSe
Lead (II) Sulfide, PbS

POCEAN09 / 104213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.