MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mueller Alloy 3450 Leaded Brass (UNS C34500)
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Used for screw machine products requiring some cold formability (i.e. crimping, knurling)

Applications: The 3450 is used for screw machine applications requiring the ability to be cold formed either during, or subsequent to, machining. The material can be thread rolled, knurled, bent, flared, swaged or staked. Alloy 3450 exhibits somewhat superior ductility in relation to comparable (i.e. alloy 3530) alloys. Typical applications include valve terms, adapters, couplings, gears, pinions, flare fittings.

Information Provided by Mueller Industries Inc.

Key Words: ASTM B453, SAE J463, UNS C34500 (Rods, Bars, Shapes and Forgings)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6666
Tensile Strength at Break 372 MPa54000 psi
Tensile Strength, Yield 234 MPa34000 psi
Elongation at Break 35 %35 %
Machinability 90 %90 %UNS C36000 = 100%
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relieving
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 62 - 65 %62 - 65 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 1.5 - 2.5 %1.5 - 2.5 %
Zinc, Zn 32.5 - 36.5 %32.5 - 36.5 %Remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-leaded brass, UNS C34200
High-leaded brass, 62%, UNS C35300
Oxygen-free Electronic Copper (OFE), UNS C10100, H00 Temper, flat products
Free-Cutting Brass, UNS C36000, H01 (Cold Drawn 15%) Temper shapes
High Leaded naval brass, UNS C48500

NMUEL900 / 97688

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.