MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for AISI 5000 Series Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 5000 Series Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "AISI 5000 Series Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 - 7.85 g/cc0.282 - 0.284 lb/in³Average value: 7.84 g/cc Grade Count:230
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 163 - 400163 - 400Average value: 253 Grade Count:209
Hardness, Knoop 188 - 369188 - 369Average value: 279 Grade Count:186
Hardness, Rockwell B 85.0 - 99.085.0 - 99.0Average value: 96.8 Grade Count:186
Hardness, Rockwell C 11.0 - 66.011.0 - 66.0Average value: 27.9 Grade Count:198
Hardness, Vickers 175 - 361175 - 361Average value: 268 Grade Count:186
Tensile Strength, Ultimate 570 - 2300 MPa82700 - 334000 psiAverage value: 1000 MPa Grade Count:199
Tensile Strength, Yield 275 - 2000 MPa39900 - 290000 psiAverage value: 739 MPa Grade Count:199
Elongation at Break 2.00 - 28.6 %2.00 - 28.6 %Average value: 17.9 % Grade Count:199
Modulus of Elasticity 200 - 210 GPa29000 - 30500 ksiAverage value: 206 GPa Grade Count:229
Bulk Modulus 160 GPa23200 ksiAverage value: 160 GPa Grade Count:187
Poissons Ratio 0.290 - 0.3000.290 - 0.300Average value: 0.292 Grade Count:228
Machinability 40.0 - 70.0 %40.0 - 70.0 %Average value: 59.8 % Grade Count:189
Shear Modulus 78.0 - 80.0 GPa11300 - 11600 ksiAverage value: 80.0 GPa Grade Count:226
Izod Impact 10.0 - 41.0 J7.38 - 30.2 ft-lbAverage value: 20.8 J Grade Count:13
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.0000228 ohm-cm0.00000200 - 0.0000228 ohm-cmAverage value: 0.0000188 ohm-cm Grade Count:226
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.9 - 14.9 µm/m-°C6.61 - 8.28 µin/in-°FAverage value: 13.6 µm/m-°C Grade Count:80
Specific Heat Capacity 0.470 - 0.519 J/g-°C0.112 - 0.124 BTU/lb-°FAverage value: 0.482 J/g-°C Grade Count:189
Thermal Conductivity 40.0 - 52.0 W/m-K278 - 361 BTU-in/hr-ft²-°FAverage value: 45.9 W/m-K Grade Count:188
Transformation Temperature 218 - 910 °C424 - 1670 °FAverage value: 622 °C Grade Count:37
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0150 - 0.100 %0.0150 - 0.100 %Average value: 0.0750 % Grade Count:3
Boron, B 0.000500 - 0.00300 %0.000500 - 0.00300 %Average value: 0.00175 % Grade Count:48
Carbon, C 0.130 - 1.10 %0.130 - 1.10 %Average value: 0.570 % Grade Count:230
Chromium, Cr 0.130 - 1.60 %0.130 - 1.60 %Average value: 0.893 % Grade Count:230
Iron, Fe 96.2 - 98.6 %96.2 - 98.6 %Average value: 97.5 % Grade Count:230
Manganese, Mn 0.200 - 1.30 %0.200 - 1.30 %Average value: 0.747 % Grade Count:230
Molybdenum, Mo 0.0600 - 0.100 %0.0600 - 0.100 %Average value: 0.0783 % Grade Count:35
Nickel, Ni 0.200 - 0.250 %0.200 - 0.250 %Average value: 0.229 % Grade Count:34
Phosphorus, P 0.0150 - 0.0350 %0.0150 - 0.0350 %Average value: 0.0328 % Grade Count:229
Silicon, Si 0.100 - 0.400 %0.100 - 0.400 %Average value: 0.230 % Grade Count:229
Sulfur, S 0.00100 - 0.0450 %0.00100 - 0.0450 %Average value: 0.0350 % Grade Count:229

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Overview of materials for AISI 9000 Series Steel
Overview of materials for AISI 6000 Series Steel
Overview of materials for AISI 8000 Series Steel
Overview of materials for Low Alloy Steel

M01001 / 81707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.