MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealability.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Agriculture Film
  • Batch Inclusion Bags
  • Coextrusion Films
  • Construction Film
  • Form Fill and Seal Packaging
  • Freezer Film
  • Heavy Duty Bags
  • Ice Bags
  • Poultry Bag
  • Produce Bags

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ExxonMobil method
Vinyl Acetate Content 6.0 %6.0 %ExxonMobil Method
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 620 %620 %ASTM D882
Elmendorf Tear Strength MD 130 g130 gASTM D1922
Elmendorf Tear Strength TD 100 g100 gASTM D1922
Dart Drop Test 490 g1.08 lbASTM D1709A
Film Tensile Strength at Break, MD 32.4 MPa4700 psiASTM D882
Film Tensile Strength at Break, TD 31.7 MPa4600 psiASTM D882
1% Secant Modulus, MD 124 MPa18000 psiASTM D882
1% Secant Modulus, TD 145 MPa21000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 102 °C<= 216 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 6.1 %6.1 %ASTM D1003
Gloss 66 %66 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene
ExxonMobil LD 07024.LQ Low Density Polyethylene Resin

PEX99229 / 175465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.