MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories HSM-35 Heat-Setting Mortar
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Grain Size 75 µm75 µm50% <= 0.075 mm
 300 µm300 µm5% >= 0.30 mm
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 2.4525 MPa
@Temperature 1400 °C,
Time 10800 sec
355.71 psi
@Temperature 2550 °F,
Time 3.00 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 - 3.00 min0.0167 - 0.0500 hourSetting Time
 
Component Elements PropertiesMetricEnglishComments
Al2O3 50 - 55 %50 - 55 %
Fe2O3 >= 3.0 %>= 3.0 %
SiO2 40 - 45 %40 - 45 %
 
Descriptive Properties
Main ApplicationsSK35 Bricks
Refractoriness (SK)35=

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories ASM-35 Air-Setting Mortar
BNZ Materials Zelie No. 20 Mortar
BNZ Materials No. 2986 Mortar

CCHOS344 / 124288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.