Description: MTM21S is a 120°C (248°F) curing, styrene free, polyester resin matrix. MTM21S has been developed specially for tube rolling applications and can be processed by oven or press molding. Features & Benefits: - Styrene-free
- 60 days out life at 21°C (70°F)
- 12 months storage at -18°C (0°F)
- 80 to 140°C (176 to 284°F) cure temperature
- Oven or press molding
Product Variants: MTM21S: natural color MTM21SMG: Medium Gray MTM21SW: WhiteNote 1: Material: MTM21S/430 g/m2 8H E-glass unidirectional tape; Cure cycle: 1 hr at 120°C (248°F), 6.2 bar (90 psi) Information provided by Cytec, subsequently acquired by Solvay. |