MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niobium (V) Oxide, Nb2O5
Categories: Ceramic; Oxide

Material Notes: White orthorhombic crystals

Key Words: Nb2O5; Niobium Pentoxide, Niobium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.60 g/cc0.166 lb/in³
Molecular Weight 265.81 g/mol265.81 g/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000100-0.0000100cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 392.4 J/g168.8 BTU/lb
Melting Point 1512 °C2754 °F
 
Descriptive Properties
CAS Number1313-96-8
ColorWhite
Crystal StructureOrthorhombic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MV Labs NB800 Nb2O5 Niobium(V) oxide
Tantalum (V) Oxide, Ta2O5
American Elements Niobium Oxide Nanoparticles
Aluminum, Al
American Elements Tantalum Oxide Nanopowder

EINOR0555 / 3684

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.