MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7076-T61
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97076; Aluminium 7076-T61; AA7076-T61; Al7076-T61
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 150150500 kg load with 10 mm ball
Hardness, Knoop 191191Converted from Brinell Hardness Value
Hardness, Rockwell A 53.553.5Converted from Brinell Hardness Value
Hardness, Rockwell B 8787Converted from Brinell Hardness Value
Hardness, Vickers 176176Converted from Brinell Hardness Value
Tensile Strength, Ultimate 510 MPa74000 psi
Tensile Strength, Yield 470 MPa68200 psi
Elongation at Break 14 %
@Thickness 1.60 mm
14 %
@Thickness 0.0630 in
In 5 cm
Modulus of Elasticity 67.0 GPa9720 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Shear Modulus 25.0 GPa3630 ksiEstimated from similar Al alloys.
Shear Strength 300 MPa43500 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000430 ohm-cm0.00000430 ohm-cmEstimated from trends in similar Al alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.6 µm/m-°C
@Temperature 20.0 - 100 °C
12.0 µin/in-°F
@Temperature 68.0 - 212 °F
 23.2 µm/m-°C
@Temperature 20.0 - 300 °C
12.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.880 J/g-°C0.210 BTU/lb-°FEstimated from trends in similar Al alloys.
Thermal Conductivity 160 W/m-K1110 BTU-in/hr-ft²-°FEstimated from trends in similar Al alloys.
Melting Point <= 630 °C<= 1170 °FEstimated from trends in similar Al alloys.
Liquidus 630 °C1170 °FEstimated from trends in similar Al alloys.
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 354 - 371 °C670 - 700 °F
Precipitation Temperature 121 °C250 °Fafter solution anneal, heat to temperature for 24 hr, air cool
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86.8 - 91.2 %86.8 - 91.2 %As remainder
Copper, Cu 0.30 - 1.0 %0.30 - 1.0 %
Iron, Fe <= 0.60 %<= 0.60 %
Magnesium, Mg 1.2 - 2.0 %1.2 - 2.0 %
Manganese, Mn 0.30 - 0.80 %0.30 - 0.80 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn 7.0 - 8.0 %7.0 - 8.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 7075-T73; 7075-T735x
Aluminum 7075-T76; 7075-T7651
Aluminum 7075-O
Overview of materials for 7000 Series Aluminum Alloy

MA7076T61 / 9598

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.