MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® 368R Crystal Clear Transparent 77851 SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Luran® 368R is a general purpose grade of SAN with well-balanced properties, suitable for injection molding and extrusion. It features very good transparency, good heat resistance and very good dimensional stability. Excellent transparency, Good surface appearance, Good chemical resistance, Good heat resistance, Very good dimensional stability. Applications: Cosmetic packaging, Water filters, Seat shell, Sanitary devices, Household appliances, Tooth brush handles

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Key Words: 368 R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³with external lubricant
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
0.20 %
@Temperature 73.4 °F
50% RH; ISO 62
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inISO 294-4
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/in
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 220 °C
10 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8383M83
Ball Indentation Hardness 165 MPa23900 psiISO 2039-1
Tensile Strength, Yield 75.0 MPa10900 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 3.70 GPa537 ksiISO 527
Flexural Strength 125 MPa18100 psiISO 178
Izod Impact, Notched (ISO)  2.00 kJ/m²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 2.00 kJ/m²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched  1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 3500 MPa508000 psiISO 899
Tensile Creep Modulus, 1000 hours 2800 MPa406000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0040
@Frequency 100 Hz
0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 106 °C
@Load 5.10 kg
223 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5691.569Sodium D Line; ISO 489
Haze <= 1.0 %<= 1.0 %ASTM D1003
Transmission, Visible >= 86 %
@Wavelength 550 nm
>= 86 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 260 °C428 - 500 °FISO 294
Mold Temperature 40.0 - 80.0 °C104 - 176 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
 
Descriptive Properties
ColorTransparent 77851
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® 358N SAN
INEOS Styrolution Luran® 378P Crystal Clear Transparent SAN
INEOS Styrolution Luran® 348Q Crystal Clear Transparent 77850 SAN
Entec Hyril® SAN500 Styrene Acrylonitrile
INEOS Styrolution Luran® 378P G7 Styrene Acrylonitrile (SAN)

PBASG0597 / 132230

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.