MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under load is excellent along with its chemical resistance to greases, oils and hydrocarbons.

Capron 8232G HS is ideally suited for applications such as safety helmet parts, washers, gears, engine and motor parts, chutes, and higher temperature environments.

Data provided by Allied Signal.

Processing: Max. water content 0.16%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 250-280 degC (482-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO data
Water Absorption 1.2 %1.2 %24 hrs; ISO data
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; 23°C; ISO data
Water Absorption at Saturation 7.1 %7.1 %in water; 23°C; ISO data
Viscosity Measurement 5050Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 170 MPa24700 psiASTM data at 5 mm/min.
 172 MPa24900 psiISO value at 5mm/min.
Elongation at Break 3.5 %3.5 %ISO, 5 mm/min
 3.5 %3.5 %ASTM, 5 mm/min
Flexural Yield Strength 270 MPa39200 psiASTM Data
Flexural Modulus 6.24 GPa905 ksiISO Value
 7.105 GPa1031 ksiASTM Value
Poissons Ratio 0.350.35ISO data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 218 °C424 °FISO data
Deflection Temperature at 1.8 MPa (264 psi) 201 °C394 °FISO data
 204 °C399 °FASTM Data
Flammability, UL94  HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
 HB
@Thickness 6.00 mm
HB
@Thickness 0.236 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 275 °C527 °FSee Materials Notes
Mold Temperature 95.0 °C203 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)
Overview of materials for Nylon 6, 20% Mineral Filled
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
A. Schulman Matrixx 75S5251 Flame Retardant 25% Glass Filled Nylon 6/6 (5VA)

PALC49 / 23843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.