MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Elix Polymers ELIX ABS M203FC Acrylonitrile Butadiene Styrene (ABS), Injection Molded
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food contact acc. to BfR and FDA, DMF registered. Easy flowing, high gloss, standard impact strength.

ISO Shortname: ISO 2580-ABS 0,MG,095-25-16-25

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in60x60x2; ISO 294-4
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in60x60x2; ISO 294-4
Melt Flow 31 g/10 min
@Load 10.0 kg,
Temperature 220 °C
31 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psiISO 2039-1
Tensile Strength, Yield 46.0 MPa6670 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 15 %>= 15 %50 mm/min; ISO 527-1,-2
Elongation at Yield 2.6 %2.6 %50 mm/min; ISO 527-1, -2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 70.0 MPa10200 psi2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.050
@Frequency 100 Hz
0.050
@Frequency 100 Hz
IEC 60250
 0.090
@Frequency 1e+6 Hz
0.090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FISO 75-1,-2
Vicat Softening Point 99.0 °C
@Load 5.10 kg
210 °F
@Load 11.2 lb
50°C/h; ISO 306
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FInjection molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secInjection molding; ISO 294
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Burning rate60 mm/minUS-FMVSS, ISO 3795, 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers ELIX ABS M205FC Acrylonitrile Butadiene Styrene (ABS), Injection Molded
Geon® Performance Solutions Vinyl Flexible XV 3716 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible XV3785 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible XV3863 Polyvinyl Chloride, Flexible
Ineos ABS Lustran® 308 ABS, Medical Grade

PELIX012 / 183327

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.