MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. It possesses thermal conductivity and very good electrical insulation values. Its softness optimizes the ability to retrieve components if needed. This can be accomplished with a sharp knife or razor blade. It has great handling properties: an easy to use two to one mix ratio by weight, good flow and a long working life. It has very low exotherm enabling it to cure many inches in depth if needed. Its hardness is very low, about 20-30 Shore A. The combination of its easy handling and cured properties enables this versatile system to be used in a variety of applications, especially the sealing of sensitive electronic parts and related components. It is particularly useful in those applications where softness and thermal conductivity are desirable. One specialty use for Super Gel 9AOND is for situations where the dampening of energy is required. The softness allows it to be easily repairable and confers it with thermal cycling and thermal and mechanical shock resistance. Super Gel 9AOND bonds well to an array of substrates, such as metals, glass, ceramics and many rubbers and plastics. It has a long working life of 6-8 hours depending on the mass that is mixed (the smaller the mass, the longer the working life). It has very good chemical resistance to water, oils and fuels. The color of both Parts A and B are light gray. After mixing, Super Gel 9AOND is a thicker paste with non-drip application properties. This multi-functional system is widely used in the aerospace, electronic, optical, electro-optical and other specialty industries where the unique blend of properties is needed.

Product Advantages:

  • Easy handling; two to one mix ratio by weight or volume; non-drip consistency
  • Very low exotherm; long working life
  • Great softness and resilience, yet solid dimensional stability
  • Easily repairable; widely used for retrieving components
  • Often used in conjunction with sensitive electronic components or when dampening is needed
  • Excellent thermal conductivity and electrical insulation properties
Key Features
  • Great for bonding and sealing
  • Convenient handling & curing at room temperature
  • Strong electrical insulation properties
  • Cures to a low Shore A hardness
  • High thermal conductivity
  • Relatively easy to remove

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.14 g/cc2.14 g/ccPart B
 2.16 g/cc2.16 g/ccPart A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 1.38 MPa>= 200 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz,
Temperature 25.0 °C
4.5
@Frequency 60 Hz,
Temperature 77.0 °F
Dielectric Strength >= 15.7 kV/mm
@Thickness 3.17 mm
>= 400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.44 - 1.59 W/m-K10.0 - 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 93.3 °C200 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 - 420 min
@Temperature 23.9 °C
4.00 - 7.00 hour
@Temperature 75.0 °F
 360 - 480 min
@Temperature 23.9 °C
6.00 - 8.00 hour
@Temperature 75.0 °F
for 48 hrs, plus 140-150°F
Pot Life 360 - 480 min360 - 480 min200 gram batch
 420 - 540 min420 - 540 min100 gram batch
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in original unopened container
 
Descriptive Properties
Mixing Ratio (A to B)2:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond Super Gel 9AO Thermally Conductive Urethane Modified Epoxy Gel
Master Bond Supreme 10AOHT Thermally Conductive One Component Epoxy System
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Master Bond EP37-3FLFAO Low Outgassing Thermally Conductive Epoxy System

PMASTB362 / 149609

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.