MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrocast 80 Lightweight Castable Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to thermal shock, and excellent resistance to attack by molten aluminum.

Applications

  • Aluminum transfer troughs
  • Insulating casting troughs
  • Wagstaff table sections

Advantages

  • Low thermal conductivity
  • Excellent thermal shock resistance
  • Non-wetting to molten aluminum
  • Light-weight

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.281 g/cc0.04628 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.00200 GPa
@Temperature 538 °C
0.290 ksi
@Temperature 1000 °F
 0.00200 GPa
@Temperature 816 °C
0.290 ksi
@Temperature 1500 °F
 0.00300 GPa
@Temperature 110 °C
0.435 ksi
@Temperature 230 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.320 W/m-K
@Temperature 260 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.360 W/m-K
@Temperature 538 °C
2.50 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.390 W/m-K
@Temperature 816 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 1500 °F
Maximum Service Temperature, Air 1204 °C2199 °F
Shrinkage 0.050 %
@Temperature 816 °C
0.050 %
@Temperature 1500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast AR LITE Castable Refractory

CPYRO160 / 1878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.