MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik DYNACOLL® 7363 Copolyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Polyester-Polyols: With its DYNACOLL® 7000 polyester-polyols Evonik offers tailor-made raw materials for one-component moisture-curable hotmelt (RHM) adhesives and sealants. DYNACOLL® 7000 products are linear copolyesters with primary hydroxyl functionality and medium molecular weight. Depending on their morphology the product range is divided into three basic groups:
  • DYNACOLL® 7300 series partially crystalline, solid
The product group is designed as a building block system, most DYNACOLL® 7000 polyester-polyols are compatible with each other. Partially incompatible but miscible systems are, however, necessary in many applications as well. DYNACOLL® 7000 copolyesters are usually supplied in 25 or 30 kg and 190 or 200 kg steel drums. Liquid bulk deliveries are available on special request.

Your benefits: Our building block system allows a precise formulation of reactive PUR hot melts with low application temperatures and high heat resistance. Basic effects on the RHM properties are:

  • DYNACOLL® 7300 series
    • shortens open time (depending on crystallinity) and lowers melt viscosity
    • increases initial strength

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³DIN 51757
Viscosity  5.0 cP
@Temperature 80.0 °C
5.0 cP
@Temperature 176 °F
DIN EN ISO 3219
 11 cP
@Temperature 130 °C
11 cP
@Temperature 266 °F
Reactive Hot Melt Data; DIN EN ISO 3219
Molecular Weight 5500 g/mol5500 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 2.0<= 2.0[mg KOH/g]; DIN EN ISO 2114
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiReactive Hot Melt Data; DIN 53 504
Elongation at Break 400 %400 %Reactive Hot Melt Data
 
Thermal PropertiesMetricEnglishComments
Melting Point 56.0 °C133 °FDIN 53765
Glass Transition Temp, Tg -60.0 °C-76.0 °FDIN 53765
Flash Point >= 300 °C>= 572 °FISO 2592
Ring & Ball Softening Point 61.0 °C142 °FReactive Hot Melt Data; DIN ISO 4625
 63.0 °C145 °FDIN ISO 4625
 
Descriptive Properties
Hydroxyl Number18-24 mg KOH/gDIN 53 240-02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® C33 PA6/66
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester
Teknor Apex Chemlon 275 Nylon 6, Copolymer Impact Modified
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
DuPont Selar® PA 3426 Nylon Barrier Resin

PEVONIL086 / 196290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.