MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistance

Information provided by Wanhua Chemical Group Co., Ltd.

Key Words: FDA 21 CFR 177.1680, 177.2600; USP VI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength 25.0 MPa3630 psiASTM D412
Elongation at Break 650 %650 %ASTM D412
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ASTM D412
300% Modulus 7.00 MPa
@Strain 300 %
1020 psi
@Strain 300 %
ASTM D412
Tear Strength 60.0 kN/m342 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether

PWANTH952 / 156375

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.