System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
ExxonMobil Exxsol™ D95 Dearomatized Fluid
Categories:
Fluid
Material Notes:
Availability: Asia Pacific, Central America, North America and South America
Appearance: Clear/Transparent Liquid
Information provided by ExxonMobil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.800
g/cc
@Temperature 15.6 °C
0.0289
lb/in³
@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity
2.67
cSt
2.67
cSt
ASTM D445
Vapor Pressure
<=
0.000133
bar
@Temperature 20.0 °C
<=
0.100
torr
@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties
Metric
English
Comments
Boiling Point
227
°C
441
°F
Initial; ASTM D86
Flash Point
96.1
°C
205
°F
Method A; ASTM D93
Descriptive Properties
Aniline Point
176°F
Method E, ASTM D611
Aromatic Content (%)
0.2
ExxonMobil Method
Dry Point
487°f
ASTM D86
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil Exxsol™ D100 Dearomatized Fluid
ExxonMobil Exxsol™ DSP100/160 Dearomatized Fluid
ExxonMobil Solvesso™ 150 Aromatic Fluid
ExxonMobil Solvesso™ 100 Aromatic Fluid
PEX99593 / 175829
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.