MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals NOVAPOL® LF-Y320-A LDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes:

Homopolymer

Features:

  • High melt strength and superior bubble stability
  • Enhances throughputs in LLDPE blends
  • Superior strength and toughness
  • Excellent shrink film characteristics

Additive Packages:

  • Base resin

Applications:

  • Industrial packaging
  • Liners
  • Shrink film
  • Blends with LLDPE

Film properties are typical of blown film extruded on a 1.5" extruder with 3" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL LF-Y320 Series resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packaging or holding food during cooking.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D 792
Thickness 38.0 microns1.50 mil
Melt Index of Compound 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 16.0 MPa2320 psiASTM D 882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiASTM D 882
Film Elongation at Break, MD 110 %110 %ASTM D 882
Film Elongation at Break, TD 450 %450 %ASTM D 882
Elmendorf Tear Strength MD 320 g320 gASTM D 1922
Elmendorf Tear Strength TD 120 g120 gASTM D 1922
Dart Drop Test 160 g0.353 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM D 882
Film Tensile Strength at Break, TD 21.0 MPa3050 psiASTM D 882
1% Secant Modulus, MD 190 MPa27600 psiASTM D 882
1% Secant Modulus, TD 230 MPa33400 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 30 %30 %ASTM D 1003
Gloss 20 %20 %@ 45°; ASTM D 2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)9NOVA Chemicals Test Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals NOVAPOL® LF-Y320-C LDPE Film Resin
LyondellBasell Petrothene® NA940000 Low Density Polyethylene, Film Data
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin

PNOVB006 / 194614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.