MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik MPEG 1005 MA W
Categories: Other Engineering Material

Material Notes: CAS No: 26915-72-0

The favorable solution property of the ether functionality is combined with the high monomer reactivity of the methacrylate functionality. Unbranched ether methacrylates behave as internal plasticizers and provide polymers with very low glass transition temperatures. Due to their low volatility, VISIOMER ETMA, THFMA and BDGMA can be used as reactive diluents for reactive systems. Long polyether side chains make the corresponding polymers water-soluble and capable of ion chelation.

Applications: Construction, emulsifiers

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 1000 g/mol1000 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C
@Pressure 0.1013 MPa
212 °F
@Pressure 14.69 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VISIOMER® Terra C17.4-MA Methacrylate Monomer
Evonik VISIOMER® MADAME™ Methacrylate Monomer
Evonik VISIOMER® MAAH

PEVONIL820 / 197024

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.