MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Aremco’s high temperature ceramic adhesives are formulated using a broad range of ceramics fillers and inorganic binders, and are ideal for bonding, potting and sealing ceramics, composites, graphite, refractory metals, quartz, and semiconductors for applications to 3200°F (1760°C).

Typical Applications:
Electrical

  • Halogen Lamps
  • Heaters
  • Igniters
  • Fiberoptics
  • Resistors
  • Solid Oxide Fuel Cells
Instruments & Sensors
  • Gas Chromatographs
  • High Vacuum Components
  • Liquid Metal Inclusion Counters
  • Mass Spectrometers
  • Oxygen Analyzers
  • Strain Gauges
  • Semiconductors
  • Temperature Probes
Mechanical
  • Ceramic Honeycombs
  • Ceramic Textiles
  • Graphite Blocks
  • Refractory Insulation
  • Sagger Plates
  • Thread-Locking

Vendors: Aremco offers a range of adhesives formulated using a broad range of ceramics fillers and inorganic binders, and are ideal for bonding, potting and sealing ceramics, composites, graphite, refractory metals, quartz, and semiconductors. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.65 - 2.70 g/cc0.0957 - 0.0975 lb/in³
Viscosity 10000 - 20000 cP10000 - 20000 cP
 
Mechanical PropertiesMetricEnglishComments
Impact Test 54.2 J40.0 ft-lbTorque Strength; curing at 1000°F
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 4.13 kV/mm105 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.20 µm/m-°C4.00 µin/in-°F
Maximum Service Temperature, Air 1760 °C3200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 50.0 - 90.0 °C122 - 194 °FApplication Temp
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
Step 1, preceded by <1 hour air set
 120 min
@Temperature 260 °C
2.00 hour
@Temperature 500 °F
Step 2
 120 min
@Temperature 371 °C
2.00 hour
@Temperature 700 °F
Step 3
Shelf Life 6.00 Month
@Temperature 4.44 - 32.2 °C
6.00 Month
@Temperature 40.0 - 90.0 °F
 
Descriptive Properties
Acid ResistanceGoodafter curing at 700°F for 2 hours
Alkali ResistanceGoodafter curing at 700°F for 2 hours
ColorTan
Moisture ResistanceGoodafter curing at 700°F for 2 hours
SolventWater
Thinner885-T

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion

CAREM26a / 138297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.