MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Cerachem™ Blanket Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: All three grades of blanket have the same excellent chemical stability compared with their raw materials: Cerafiber, Cerachem Fiber and Cerachrome Fiber spun bulk. They have excellent strength before and after heating. They have superior acoustic as well as thermal insulation characteristics. The wide range of available densities and thicknesses allow for the most effective deployment of the superior thermal characteristics in a wide variety of applications.

Applications:

  • Furnace and kiln linings
  • Boiler insulations
  • Heat treatment temperature control
  • Glass furnace crown insulation
  • Furnace door seals
  • Duct linings
  • Pipe insulations
  • Thermal barriers for automotive industry
  • Insulation for field stress relieving of welds
  • High temperature filter media
  • Nuclear insulation applications
  • Steam and gas turbines insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0640 - 0.160 g/cc0.00231 - 0.00578 lb/in³4 densities available; EN 1094-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.0300 MPa4.35 psiat 64 kg/m3; EN 1094-1
 0.0700 MPa10.2 psiat 96 kg/m3; EN 1094-1
 0.0900 MPa13.1 psiat 128 kg/m3; EN 1094-1
 0.110 MPa16.0 psiat 160 kg/m3; EN 1094-1
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1090 °C
0.270 BTU/lb-°F
@Temperature 1990 °F
Thermal Conductivity  0.0600 W/m-K
@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 392 °F
at 96kg/m3
 0.0600 W/m-K
@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 392 °F
at 128kg/m3
 0.0700 W/m-K
@Temperature 200 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 392 °F
at 64kg/m3
 0.0900 W/m-K
@Temperature 400 °C
0.625 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 160kg/m3
 0.100 W/m-K
@Temperature 400 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 128kg/m3
 0.110 W/m-K
@Temperature 400 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 96kg/m3
 0.120 W/m-K
@Temperature 400 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 752 °F
at 64kg/m3
 0.130 W/m-K
@Temperature 600 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 160kg/m3
 0.150 W/m-K
@Temperature 600 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 128kg/m3
 0.160 W/m-K
@Temperature 600 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 96kg/m3
 0.180 W/m-K
@Temperature 800 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 160kg/m3
 0.200 W/m-K
@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 128kg/m3
 0.200 W/m-K
@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1110 °F
at 64kg/m3
 0.230 W/m-K
@Temperature 800 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 96kg/m3
 0.250 W/m-K
@Temperature 1000 °C
1.74 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 160kg/m3
 0.270 W/m-K
@Temperature 1000 °C
1.87 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 128kg/m3
 0.300 W/m-K
@Temperature 800 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 1470 °F
at 64kg/m3
 0.320 W/m-K
@Temperature 1000 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 96kg/m3
 0.430 W/m-K
@Temperature 1000 °C
2.98 BTU-in/hr-ft²-°F
@Temperature 1830 °F
at 64kg/m3
Shrinkage  1.0 %
@Temperature 1200 °C,
Time 86400 sec
1.0 %
@Temperature 2190 °F,
Time 24.0 hour
isothermal
 2.0 %
@Temperature 1300 °C,
Time 86400 sec
2.0 %
@Temperature 2370 °F,
Time 24.0 hour
isothermal
 3.5 %
@Temperature 1400 °C,
Time 86400 sec
3.5 %
@Temperature 2550 °F,
Time 24.0 hour
isothermal
 
Component Elements PropertiesMetricEnglishComments
Al2O3 35 %35 %
CaO+MgO 0.090 %0.090 %
K2O+Na2O 0.10 %0.10 %
Other 0.15 %0.15 %Fe2O3+TiO2
SiO2 50 %50 %
ZrO2 15 %15 %
 
Descriptive Properties
Classification Temperature (°C)1425
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Papers AZS Paper Ceramic Fiber
Morgan Advanced Ceramics Cerafelt Refractory Fiber Felt

CMORF70141 / 203439

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.