MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovako 30CrNiMo8 (6507) EN 10083-2:2006 Steel, Quenching
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Quenching and tempering steel with a very high hardenability.

Information provided by Ovako

Key Words: 1.6580, 823M30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  1000 - 1200 MPa
@Thickness 100 - 150 mm
145000 - 174000 psi
@Thickness 3.94 - 5.91 in
Round bar
 1100 - 1300 MPa
@Thickness 40.0 - 100 mm
160000 - 189000 psi
@Thickness 1.57 - 3.94 in
Round bar
 1250 - 1450 MPa
@Thickness 25.0 - 40.0 mm
181000 - 210000 psi
@Thickness 0.984 - 1.57 in
Round bar
Tensile Strength, Yield  >= 800 MPa
@Thickness 100 - 150 mm
>= 116000 psi
@Thickness 3.94 - 5.91 in
Reh, Round bar
 >= 900 MPa
@Thickness 40.0 - 100 mm
>= 131000 psi
@Thickness 1.57 - 3.94 in
Reh, Round bar
 >= 1050 MPa
@Thickness 25.0 - 40.0 mm
>= 152000 psi
@Thickness 0.984 - 1.57 in
Round bar
Elongation at Break  40 %
@Thickness 25.0 - 40.0 mm
40 %
@Thickness 0.984 - 1.57 in
Round bar
 45 %
@Thickness 40.0 - 100 mm
45 %
@Thickness 1.57 - 3.94 in
Round bar
 50 %
@Thickness 100 - 150 mm
50 %
@Thickness 3.94 - 5.91 in
Round bar
Reduction of Area  40 %
@Thickness 25.0 - 40.0 mm
40 %
@Thickness 0.984 - 1.57 in
Round bar
 45 %
@Thickness 40.0 - 100 mm
45 %
@Thickness 1.57 - 3.94 in
Round bar
 50 %
@Thickness 100 - 150 mm
50 %
@Thickness 3.94 - 5.91 in
Round bar
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
Impact Test  27.0 J
@Thickness 40.0 - 100 mm,
Temperature -40.0 °C
19.9 ft-lb
@Thickness 1.57 - 3.94 in,
Temperature -40.0 °F
Round bar
 27.0 J
@Thickness 100 - 150 mm,
Temperature -40.0 °C
19.9 ft-lb
@Thickness 3.94 - 5.91 in,
Temperature -40.0 °F
Round bar
 30.0 J
@Thickness 25.0 - 40.0 mm,
Temperature 20.0 °C
22.1 ft-lb
@Thickness 0.984 - 1.57 in,
Temperature 68.0 °F
Round bar
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 309 °C588 °FMS
 731 °C1350 °FAC1
 788 °C1450 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.26 - 0.34 %0.26 - 0.34 %
Chromium, Cr 1.8 - 2.2 %1.8 - 2.2 %
Iron, Fe 93.5 - 95.34 %93.5 - 95.34 %As Balance
Manganese, Mn 0.50 - 0.80 %0.50 - 0.80 %
Molybdenum, Mo 0.30 - 0.50 %0.30 - 0.50 %
Nickel, Ni 1.8 - 2.2 %1.8 - 2.2 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.035 %<= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Ovako 34CrNiMo6 6499 Steel, +QT
Ovako 30CrNiMo8 (6507) ISO 683-2:2016 Steel, +AR
Ovako 30CrNiMo8 EN10083-3:2006 Steel
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

NOVAKO228 / 234527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.