MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond FS152C Clear Low Viscosity Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND FS152C is a low viscosity epoxy system containing no solvents, cures at room temperature and has excellent flow and wetting characteristics. This two-part adhesive mixes easily and develops strong, durable, tough bonds to most clean, dry material surfaces including metals, ceramics, glass, wood and many plastics. Its low viscosity readily facilitates bubble release and degassing, and it has a surface dry time of 6 hours at room temperature.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 700 cP
@Temperature 25.0 °C
700 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7676
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
32.2 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Pot Life 60 min60 min
 
Descriptive Properties
Color Clear
Mix Ratio, parts by weight100/30Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 832-5 Flexible Epoxy

PTRAC270 / 71198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.