MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Monprene® OM-10240-02 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-10240-02 is designed for overmolding applications like grips and anti-skid parts for consumer/industrial products. Monprene OM-10240-02 is a low hardness, low density, translucent grade that exhibits excellent adhesion to PC, ABS, and PC/ABS.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: High Flow; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Slip; Without Fillers

Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  40
@Time 5.00 sec
40
@Time 0.00139 hour
Injection Molded; ASTM D2240
 42
@Time 1.00 sec
42
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.32 MPa916 psiDie C, 20 in/min, Flow; ASTM D412
 9.79 MPa1420 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.765 MPa
@Strain 100 %
111 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 1.63 MPa
@Strain 300 %
237 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 1.81 MPa
@Strain 100 %
263 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 4.17 MPa
@Strain 300 %
605 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 510 %510 %Die C, 20 in/min, Flow; ASTM D412
 590 %590 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 19.6 kN/m112 pliDie C, 20 in/min, Flow; ASTM D624
 32.4 kN/m185 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set 22 %
@Temperature 22.8 °C,
Time 79200 sec
22 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 232 °C360 - 450 °F
Middle Barrel Temperature 188 - 238 °C370 - 460 °F
Front Barrel Temperature 193 - 243 °C380 - 470 °F
Nozzle Temperature 199 - 249 °C390 - 480 °F
Melt Temperature 199 - 249 °C390 - 480 °F
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Monprene® OM-10240 Thermoplastic Elastomer

PTEKNQ0895 / 237386

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.