MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Sarlink® TPV X5725B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 5700B Series are highly engineered extrusion-grade thermoplastic vulcanizates with outstanding UV stability designed for demanding automotive interior and exterior sealing applications, including glass run channels, waistbelts, weather strips, seals and other profiles. This product is a low hardness, low density, high performance grade with low fogging and excellent color retention and elastic properties.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Processability; Low Density; Low Specific Gravity; Low Hardness; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Viscosity 140 cP
@Shear Rate 206 1/s,
Temperature 200 °C
140 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  23
@Time 5.00 sec
23
@Time 0.00139 hour
Extruded; ISO 868
 26
@Time 5.00 sec
26
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 1.50 MPa218 psiFlow; ISO 37
 2.50 MPa363 psiAcross Flow; ISO 37
 1.64 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
238 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air at 168 hr; ISO 188
 1.64 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
238 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air at 168 hr; ISO 188
Tensile Stress at Strain  0.500 MPa
@Strain 100 %
72.5 psi
@Strain 100 %
Across Flow; ISO 37
 1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
Flow; ISO 37
 0.465 MPa
@Strain 100 %,
Treatment Temp. 135 °C
67.4 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
 0.465 MPa
@Strain 100 %,
Treatment Temp. 150 °C
67.4 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
Elongation at Break 200 %200 %Flow; ISO 37
 520 %520 %Across Flow; ISO 37
 395 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
395 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air at 168 hr; ISO 188
 426 %
@Treatment Temp. 150 °C,
Time 605000 sec
426 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air at 168 hr; ISO 188
Tear Strength 8.94 kN/m51.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  10 %
@Temperature 22.8 °C,
Time 79200 sec
10 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 20 %
@Temperature 70.0 °C,
Time 79200 sec
20 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 51 %
@Temperature 125 °C,
Time 252000 sec
51 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV 5765B Thermoplastic Vulcanizate

PTEKNQ1207 / 237698

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.