MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Features

Modified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complicated mouldings. It is stabilized against the impact of UV radiation by the UV stabilizer on the HALS basis. Application: external use for stadium seats with guaranteed operating life of the mechanical and surface properties. Delivered in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³STN 64 0111
Linear Mold Shrinkage 0.022 cm/cm0.022 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.025 cm/cm0.025 in/inSTN 64 0808
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiSTN EN ISO 527-2
Elongation at Break 200 %200 %STN EN ISO 527-2
Tensile Modulus 1.40 GPa203 ksiSTN EN ISO 527-2
Flexural Strength 40.0 MPa5800 psiSTN EN ISO 178
Flexural Modulus 1.10 GPa160 ksiSTN EN ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
STN EN ISO 179
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FSTN EN ISO 75/A
Vicat Softening Point 114 °C237 °FB; STN EN ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Injection Pressure 60.0 - 70.0 MPa8700 - 10200 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film
Techmer ES Plastiblend® ABS 8004 UV
Techmer ES HiFill FR® ABS FR UV BK
Techmer ES HiFill FR® ABS FR UV
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized

PPLACO067 / 106945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.