MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek LUMIFELT AL20 High Temperature Kevlar® Felt
Categories: Polymer; Thermoset; Aramid

Material Notes: Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and good holding strength to maintain product integrity.

Applications

  • Insulating pads for high-temperature glass transfer applications
  • Sealing materials for annealing furnace of nonferrous metal
  • Heat shields for furnace doors
  • Cushioning material for hot glass transfer and conveyance
  • Insulating pads for conveyor line and shock absorber
  • Covering material for conveyor rolls

Advantages

  • Asbestos-free
  • Excellent heat and abrasion resistance
  • High elasticity
  • Long life to cyclic loading
  • Good recovery from compression
  • Light weight
  • Good coefficient of friction
  • Will not damage nor blur the surface of glass containers or other high-temperature glass products
  • Porosity reduces the temperature difference between pad contacting and non-contacting surfaces

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.400 g/cc0.0145 lb/in³
Permeability 1.1
@Thickness 10.0 mm
1.1
@Thickness 0.394 in
cc/sec/cm2, Air
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.9807 MPa142.2 psito 25% compression
Coefficient of Friction, Static 0.240.24
Abrasion 0.830.83Thickness reduction after 10,000 abrasion cycles under 500 g/cm2 load at 400°C
 0.900.90Thickness reduction after 10,000 abrasion cycles under 500 g/cm2 load at 320°C
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.150 W/m-K1.04 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek LUMIFELT AL20L High Temperature Kevlar® Felt
DuPont™ Kevlar® 49 Aramid Fiber
DSM Dyneema® HB212
DSM Dyneema® HB26
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

PPYRO158 / 58409

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.