MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell Ensolite™ AFM-ESD Foam Mat
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Ensolite® AFM-ESD is an engineered foam for use in anti-fatigue mats with electrostatic dissipative properties. This mat material is ideal for hospitality or transportation settings or industrial and electronics environments where sensitive equipment is in use.
  • Anti-Fatigue/Dissipative/Anti-Static
    • Built-in static resistance lowers risk of shock or damage to electronic equipment
    • Density and firmness designed for prolonged cushioning
    • Available with an anti-microbial additive for increased mold resistance
  • Long-lasting Durability
    • The closed-cell, vinyl nitrile rubber blend material is durable and long lasting
    • Moisture resistant, chemical resistant, wipes clean
    • Tested to withstand repeated impacts without loss of performance or comfort
  • Customizable
    • Uniform surface accepts printing
    • Several embossing patterns available
    • Edges can be cut or beveled for smooth transitions
    • Excellent adhesion to other substrates
Recommended Applications:
  • Hospitality
  • Industrial / Pharmaceutical
  • Aviation / Transportation
  • Electronic Assembly Production
  • Computer Room / Data Center
  • Fiber Optics Manufacturing

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.192 - 0.288 g/cc0.00694 - 0.0104 lb/in³ASTM D1056
Water Absorption <= 5.0 %<= 5.0 %ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.689 MPa>= 100 psiASTM D412
Elongation at Break >= 75 %>= 75 %ASTM D412
Compressive Strength 0.0414 - 0.0827 MPa
@Strain 25 %
6.00 - 12.0 psi
@Strain 25 %
ASTM D1056
 
Descriptive Properties
ColorBlack
Flammability0 Burn RateFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Foam Grade
Aurora Plastics GE-960F PVC/Nitrile Alloy
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Aurora Plastics TufFlex™ GF 1815 PVC/Nitrile Alloy
Armacell Ensolite™ MLC-Black PVC/NBR

PARMD057 / 186668

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.