MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Syncure™ V0030G RoHS Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.

Gel, Torque, and Dispersion were measured on a 100 phr S1025A / 20 phr V0030G Syncure System. Cured for 6 hours in water at 90°C for Gel test. Torque is > 1400. Dispersion is Visual. Pellet appearance is 1/8 round.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.11 g/cc2.11 g/ccASTM D792
Density 1.18 g/cc0.0426 lb/in³Geon® 1169; Internal Method
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Gel Content70%ASTM D2765; Crosslinked PE, Method A (Referee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Regional AvailabilityNorth America
RoHS ComplianceRoHS Compliant
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable
Avient Syncure™ S1075A Polyethylene, Crosslinked (XLPE)
Avient Syncure™ V0022G RoHS Polyethylene, Crosslinked (XLPE)
Avient Syncure™ S1000B Polyethylene, Crosslinked (XLPE)
Avient Syncure™ V0044G-UV RoHS Natural Polyethylene, Crosslinked (XLPE)

PH0POL0839 / 145408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.