MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lupolen 5261Z Q456 High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Lupolen 5261Z Q456 is a high density polyethylene (HDPE) powder with high melt viscosity for ram extrusion of peroxide cross linked pipes (PE-Xa). It is also used for compression molded plates. Applications: Drinking Water Pipe, Plumbing, Heating & Cooling

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ISO 1183-1
Melt Flow 2.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
2.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
measured on powder; ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65
@Time 3.00 sec
65
@Time 0.000833 hour
ISO 868
Ball Indentation Hardness 52.0 MPa7540 psiISO 2039-1
Tensile Strength, Yield 27.0 MPa3920 psi50mm/min; ISO 527-1,-2
Elongation at Yield 9.0 %9.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1.10 GPa160 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FISO 3146
Vicat Softening Point 80.0 °C176 °FB50; ISO 306
 132 °C270 °FA50N; ISO 306
 
Descriptive Properties
Processing MethodCompression Molding, Pipe, Sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Soil, Average
Bostik NeverSeal™ Grout
LyondellBasell Lupolen 5261Z Q456 B High Density Polyethylene (HDPE), Pipe Grade
Braskem GM8250T HDPE High Density Extrusion Polyethylene
Braskem GM7040G HDPE High Density Extrusion Polyethylene

PEQT8574 / 220209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.