MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bohler-Uddeholm UDDEHOLM RAMAX® LH Plastic Mold Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Uddeholm Ramax LH is a new chromium alloyed stainless holder steel, which is supplied in the hardened and tempered condition.

RAMAX® LH is characterized by:

  • Excellent machinability
  • Good corrosion resistance
  • Good hardenability
  • Uniform hardness in all directions
  • Good indentation resistance
Applications
  • Holders/bolsters for plastic moulds
  • Plastic and rubber moulds with low requirements on polishability
  • Die and calibers for plastic extrusion
  • Constructional parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³hardened and tempered to 350 HB
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 290290Hardened and tempered (Delivery condition)
 270 - 310270 - 310
Tensile Strength, Ultimate 1010 MPa147000 psi(hardened to 302 HB)
 903 MPa
@Temperature 199 °C
131000 psi
@Temperature 390 °F
(hardened to 302 HB)
Tensile Strength, Yield 862 MPa
@Strain 0.2 %
125000 psi
@Strain 0.2 %
68°F (hardened to 302 HB)
 772 MPa
@Strain 0.2 %,
Temperature 199 °C
112000 psi
@Strain 0.2 %,
Temperature 390 °F
hardened to 302 HB
Elongation at Break 13 %13 %(hardened to 302 HB)
 13 %
@Temperature 199 °C
13 %
@Temperature 390 °F
hardened to 302 HB
Reduction of Area  43 %
@Temperature 199 °C
43 %
@Temperature 390 °F
hardened to 302 HB
 45 %
@Temperature 20.0 °C
45 %
@Temperature 68.0 °F
hardened to 302 HB
Modulus of Elasticity 210 GPa30500 ksi68°F, (hardened and tempered to 302 HB)
 200 GPa
@Temperature 199 °C
29000 ksi
@Temperature 390 °F
hardened and tempered to 302 HB
Impact Test 180 J133 ft-lbunnotched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C
@Temperature 199 °C
6.10 µin/in-°F
@Temperature 390 °F
hardened and tempered to 302 HB
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
hardened and tempered to 302 HB
Thermal Conductivity 24.0 W/m-K
@Temperature 199 °C
167 BTU-in/hr-ft²-°F
@Temperature 390 °F
hardened and tempered to 302 HB
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.12 %0.12 %
Chromium, Cr 14 %14 %
Iron, Fe 82.64 %82.64 %as balance
Manganese, Mn 1.45 %1.45 %
Molybdenum, Mo 0.20 %0.20 %
Nickel, Ni 0.36 %0.36 %
Silicon, Si 1.0 %1.0 %
Sulfur, S 0.13 %0.13 %
Vanadium, V 0.10 %0.10 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
Bohler-Uddeholm M238 VMR® P20 Plastic Lens Mold Steel
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel

NBUCOR26 / 15495

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.