MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Supreme Petrochem SP 256 Toughened Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Characteristics
  • Superior flexibility
  • Good ball drop strength
  • Excellent clarity
  • Easy flow
Processing
  • Injection molding
Applications
  • Transparent hangers
  • Stationery items like pen barrels, geometric instruments
  • Medical products
  • Appliance parts
  • Toys and fashion accessories
  • Caps for spray cans
Material Status: Commercial : Active

Agency Ratings: FDA 21 CFR 177.1640

Information provided by Supreme Petrochem LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.3 MPa4970 psi50 mm/min; ASTM D638
Elongation at Break 10 %10 %50 mm/min; ASTM D638
Flexural Strength 46.1 MPa
@Thickness 3.20 mm
6690 psi
@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.72 GPa
@Thickness 3.20 mm
249 ksi
@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 2.75 J/cm
@Thickness 3.20 mm
5.15 ft-lb/in
@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 2.75 J/cm
@Thickness 3.20 mm
5.15 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
Vicat Softening Point 98.0 °C208 °F1kg load; 120°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %
@Thickness 1.00 mm
1.0 %
@Thickness 0.0394 in
SPL test method
Transmission, Visible 88 %
@Thickness 1.00 mm
88 %
@Thickness 0.0394 in
SPL test method
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 220 °C<= 428 °F
Mold Temperature 40.0 - 50.0 °C104 - 122 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-ABS 3365 High Impact ABS
Supreme Petrochem SC 6501 Toughened Polystyrene
Americas Styrenics Styron® 482 High Impact Polystyrene
Dow AIM® 4810 High Impact Styrenic Resin
Dow AIM® 4800 High Impact Styrenic Resin

PSUP29 / 69461

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.