MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay IGEPAL® CO 630 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Nonyl phenol ethoxylate (9 mole EO). Good emulsifier and wetter. All-purpose detergents. Used in acid cleaners, detergent sanitizers and dedusting agents.

Chemical Name: ETHOXYLATED NONYLPHENOL, BRANCHED

CAS: 68412-54-4

Available in: Asia Pacific, Europe, Latin America and North America

Applications: IGEPAL© CO-630 is a Nonionic co-emulsifier used in emulsion polymerization and also widely used as a wetting agent in different formulations. Hard Surface Cleaners, Laundry Detergent Liquids, Miscellaneous Cleaners, Oil based fluids, Polyacrylamide Emulsions

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Surface Tension 32 dynes/cm32 dynes/cmat CMC
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy LiquidRP-0064
Cloud point52-56°C1% Solution, RP-0124
Color<50APHA, RP-0134
Critical Micelle Concentration (%)0.005
HLB number13
Ionic ChargeNonionic
Moles of Ethylene Oxide9
Neutralization Number<0.5 mg KOH/gpH7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay IGEPAL® CA 210 Surfactant
Solvay IGEPAL® BC/4 Surfactant
Solvay GEROPON® T-22 A Surfactant
Solvay GEROPON® T/36 Surfactant
Solvay GEROPON® T/36 DF Surfactant

WRHOD147 / 137378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.