MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Categories: Ceramic; Carbide; Ceramic Matrix Composite

Material Notes: Engineered ceramic composite structures for a broad range of industries and applications.

Reinforcing Fiber Flexibility: S300 - Sylramic SiC
Preceramic Polymer Matrix Precursors: S300 - Crystalline (SiC + Si3N4) or SiC
Physical Attributes: Dense Matrix (<5%), High Temperature Capability, Good Matrix Dominated Properties and Wear Resistance

Typical Applications: Commercial Aviation Exhaust, Military Aircraft Propulsion Exhaust, Industrial

Produced using the Polymer Impregnation & Pyrolysis (PIP) process. This versatile and robust process is well suited for the fabrication of complex components. The PIP process utilizes a combination of polymeric and ceramic processes, combining a variety of ceramic fibers, fillers and pre-ceramic polymer resins to produce engineered ceramic composite structures for a broad range of industries and applications.

Process temperatures referenced in property table: T1< T2 < T3 < T4.

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress at Strain  75.8 MPa
@Strain 0.05 %
11000 psi
@Strain 0.05 %
Process Temperature T4
 75.8 MPa
@Strain 0.05 %
11000 psi
@Strain 0.05 %
Process Temperature T1
 82.7 MPa
@Strain 0.05 %
12000 psi
@Strain 0.05 %
Process Temperature T2
 89.6 MPa
@Strain 0.05 %
13000 psi
@Strain 0.05 %
Process Temperature T3
 138 MPa
@Strain 0.1 %
20000 psi
@Strain 0.1 %
Process Temperature T4
 145 MPa
@Strain 0.1 %
21000 psi
@Strain 0.1 %
Process Temperature T1
 148 MPa
@Strain 0.1 %
21500 psi
@Strain 0.1 %
Process Temperature T2
 159 MPa
@Strain 0.1 %
23000 psi
@Strain 0.1 %
Process Temperature T3
 183 MPa
@Strain 0.15 %
26500 psi
@Strain 0.15 %
Process Temperature T4
 193 MPa
@Strain 0.15 %
28000 psi
@Strain 0.15 %
Process Temperature T1
 200 MPa
@Strain 0.15 %
29000 psi
@Strain 0.15 %
Process Temperature T2
 214 MPa
@Strain 0.15 %
31000 psi
@Strain 0.15 %
Process Temperature T3
 228 MPa
@Strain 0.2 %
33000 psi
@Strain 0.2 %
Process Temperature T4
 241 MPa
@Strain 0.2 %
35000 psi
@Strain 0.2 %
Process Temperature T1
 248 MPa
@Strain 0.2 %
36000 psi
@Strain 0.2 %
Process Temperature T2
 262 MPa
@Strain 0.2 %
38000 psi
@Strain 0.2 %
Process Temperature T3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Silicon Carbide, Reaction-Bonded, SiSiC
Morgan Advanced Ceramics CVD Silicon Carbide
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
CeramTec Rocar® ST Silicon Carbide, SSiC

CCOIC007 / 122047

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.