MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, seafood and cheese packaging; Coextrusions with nylon or in other film structures as a heat seal

Data provided by the manufacturer, DuPont Packaging.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 460 %460 %ASTM D882
Film Elongation at Break, TD 450 %450 %ASTM D882
Secant Modulus, MD 0.160 GPa23.2 ksiASTM D882
Secant Modulus, TD 0.0450 GPa6.53 ksiASTM D882
Impact 410410Spencer Impact in J/cm; ASTM D3420
Elmendorf Tear Strength, MD 1.10 g/micron27.9 g/mil
Elmendorf Tear Strength, TD 1.40 g/micron35.6 g/mil
Dart Drop 22.1 g/micron561 g/milASTM D1709B
Seal Strength <= 3400 g/25 mm<= 3400 g/inVaries with seal bar temp.
Hot Tack Strength <= 3000 g/25 mm<= 3000 g/inVaries with seal bar temp.; Packforsk Method
Film Tensile Strength at Break, MD 41.0 MPa5950 psiASTM D882
Film Tensile Strength at Break, TD 35.0 MPa5080 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 95.0 °C203 °FDSC; ASTM D3418
Vicat Softening Point 70.0 °C158 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 100 %100 %20°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C376 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1650SB

PDU619 / 33096

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.